NEW SALE

FINOLLOY CoCr Solder

Picture may vary from actual product.
Item number 42009
4,5 g

available, in stock

For all CoCr alloys.
Physical data:
    Melting range 1100-1150 °C; working temperature 1180 °C.
Composition in %:
    Co 61.0; Cr 28.5; Si 4.2; Mo 3.1; B 1.5; Fe 1.3; C < 1.0.