FINOLLOY CoCr Solder








Picture may vary from actual product.
Item number
42009
4,5 g
Please log in to see the price information
available, in stock
For all CoCr alloys.
4.5 g
Physical data:
- Melting range 1100-1150 °C; working temperature 1180 °C.
Composition in %:
- Co 61.0; Cr 28.5; Si 4.2; Mo 3.1; B 1.5; Fe 1.3; C < 1.0.
4.5 g
Last seen products
Heatless Grinding Discs, ø 22 x 3 mm
available, in stock
partially in stock
Item no.: 67205
50 pieces